Metal stitching
Cold metal stitching of cracked castings such as engine blocks and housings. A crack repair without welding and without heat input into the casting.
Repair the crack without welding.
Metal stitching is a cold repair method for cracked castings. Stitching elements are locked across the crack to close it and hold it, without the heat input that welding introduces.
Repaired where it is installedEngine blocks and housings
Cracked engine blocks and housings, and other castings where heat input is a concern.
A cold alternative to welding
Because the repair is cold, no weld heat goes into the casting. Whether stitching or another route suits the job depends on the casting, the crack and the loads on it.
When stitching is not the answer
Where the assessment shows another repair route is better for the casting, we say so when we recommend the route.
Assessment first
A crack repair starts with understanding the crack, its cause where it can be established, and the casting. A recommendation not to repair, or to replace the component, can be a valid outcome.
What the work covers.
Every job is scoped to the component and the result you need. A typical scope includes:
- Assessment of the crack, the casting and its operating conditions
- Inspection to establish the extent of the crack before repair, where needed
- Cold stitching repair of the cracked casting
- Final checks and a record of the completed repair
We agree the scope with you before work starts. Not every component suits every repair route, and we say so when it does not.

Assessed, agreed, machined, verified.
We assess the condition
Measurements, inspection and the history of the component, before any material is removed.
We agree the scope
The repair route, tolerances and acceptance criteria are agreed with you, together with schedule and price.
We machine in place
Portable equipment is set up around the component, at the vessel, platform, yard or plant.
We verify and document
Final dimensions are measured and recorded, and you receive closeout documentation with photographs.
Send us what you have.
You do not need every answer before you call. These details help us scope the job and quote it accurately.
- 01Casting type, material where known and the location of the crack
- 02Photographs, measurements and any inspection findings
- 03Operating conditions, the loads on the casting and the repair outcome required
Questions about metal stitching.
Straight answers to what superintendents, engineers and plant managers ask before they call.
01What if stitching is not suitable?
Then we tell you, and explain which repair route fits the casting, the crack and the loads better.
02Can a cracked engine block be repaired without welding?
Often a cold stitching repair is an option. It depends on the casting, the position and extent of the crack and the loads it carries. We assess before we recommend a route.
03Does stitching put heat into the casting?
No. Stitching is a cold process, so it does not introduce weld heat into the casting.
04What should we send to start the discussion?
Photographs of the crack, the component and its location, any measurements or inspection reports, and the operating conditions.
Discuss your metal stitching job.
Send what you know. We review it with you and help identify the practical next step.
Equipment down: WhatsApp us, answered 24/7. Planned work: we reply the same business day.